Drops of a solution of acid are placed on the specimen, the surface of which is rubbed gently with a glass rod to ensure penetration. The changes in colour of the textile, while it is still wet and after drying, are assessed with the grey scale. Three tests differing in severity are provided.
WITHDRAWN
ISO 105-E05:1989
95.99
Withdrawal of Standard
Jun 21, 2006
Corrected by
ISO 105-E05:1989/Cor 1:2002
WITHDRAWN
ISO 105-E05:2006