Specifies the method of Knoop hardness test covering test forces up to and including 9,807 N. The principle of the method is forcing a diamond indenter, in the form of a rhombic-based pyramid with specified angles between opposite faces at the vertex, into the surface of a test piece and measuring the long diagonal of the indentation left in the surface after removal of the test force. The Knoop hardness is proportional to the quotient obtained by dividing the test force by the projected area of the indentation.
WITHDRAWN
ISO 4545:1993
95.99
Withdrawal of Standard
Nov 17, 2005
WITHDRAWN
ISO 4545-1:2005
Only informative sections of projects are publicly available. To view the full content, you will need to members of the committee. If you are a member, please log in to your account by clicking on the "Log in" button.